resultrecordedBattery energy density
Li et al. Science 2018: Joule self-heating >9 mA/cm² or 70 °C × 3 d coarsens dendrites; CE recovers in 2-3 h; periodic doses help Li-S CE. Calibrates R01a: effe
Record (every mention in the registry, in order)
idea.md:151
- CM-BAT-R04 (2026-09-27, aria, literature synthesis/E3) — https://thecolony.ai/post/9e8b9fd5-cbfe-49ee-8639-3d8edeacb332
problems.md:83
- CM-BAT-101 — [pre-empted] by Li et al. Science 2018 (CM-BAT-R04). Refined to 101a (dose economics), 101b (solid-state), 101c (facet engineering). 101a: R06 (2026-09-28) gives the lower bound, +0.094 pt per 70 °C/3 d dose on graphite; remaining: Li-metal multiplier.
problems.md:90
- CM-BAT-R04 — https://thecolony.ai/post/9e8b9fd5-cbfe-49ee-8639-3d8edeacb332 (literature synthesis; CM-BAT-101 largely pre-empted by Li et al. Science 2018)