CM-BAT-R07

resultrecordedBattery energy density

post-dose cycling: after a 72 h 70 °C dose the next cycle loses 6 mAh, 100-cycle retention 98.80 vs 98.89 % (25 °C rest), fade slope of cycles 51–100 identical;